Various welding methods  are applicable in the same manner as with the standard austenitic stainless  steels, including shielded metal arc welding, TIG welding, and plasma welding.  Susceptibility of Inconel 625/UNS N06625/2.4856 Alloy/ASTM B443 to  solidification cracking is higher than that of Type 304 and lower than that of  Type 310S. 
Welding of Inconel 625/UNS  N06625/2.4856 Alloy/ASTM B443 can be accomplished by the gas-shielded processes  using a tungsten electrode or a consumable electrode. Post weld heat treatment  of the weld is not necessary to maintain corrosion resistance. Heavy restrained  sections can be welded and the weld's mechanical properties follow the same  trends as base metal properties. Standard practices such as clean surfaces,  good joint alignment, U-joints for thicker sections, etc., should be followed. 
                               |